Ebook: Stress-Corrosion Cracking. Materials Performance and Evaluation
- Tags: Stress corrosion. Alloys -- Stress corrosion. Corrosion sous tension. Alliages -- Corrosion sous-tension. SCIENCE -- Nanoscience.
- Year: 1992
- Publisher: ASM International
- City: Materials Park, Ohio
- Edition: illustrated edition
- Language: English
- pdf
Contents include: Complete coverage of SCC for a variety of materials and SCC in different environments: carbon and low-alloy steels high-strength steels stainless steels nickel-base alloys copper alloys aluminum alloys magnesium alloys titanium alloys zirconium alloys uranium alloys amorphous alloys glasses and ceramics weldments in boiling water reactor service